X8Cr Ni S18-9建筑用耐腐蝕鋼棒材
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
牌號:X8Cr Ni S18-9
|
|
|
|
|
|
|
|
|
|
編號:1.4305
|
|
|
|
|
|
|
|
|
|
分類:奧氏體不銹鋼
|
|
|
|
|
|
|
|
|
|
密度:7.9 g/cm3
|
|
|
|
|
|
|
|
|
|
標(biāo)準(zhǔn):
|
|
|
|
|
|
|
|
|
|
EN 10088-2:2005不銹鋼。通用耐腐蝕鋼片/板和帶材交貨技術(shù)條件
|
|
|
|
|
|
|
|
|
|
EN 10088-3:2005不銹鋼。一般用途耐腐蝕鋼的半成品、棒材、線材、型材和光亮產(chǎn)品的交貨技術(shù)條件
|
|
|
|
|
|
|
|
|
|
EN 10297-2:2005機(jī)械和一般工程用無縫圓形鋼管。不銹鋼。技術(shù)交付條件
|
|
|
|
|
|
|
|
|
|
EN 10088-1:2005不銹鋼。不銹鋼清單
|
|
|
|
|
|
|
|
|
|
EN 10088-5:2009不銹鋼。建筑用耐腐蝕鋼棒材、棒材、線材、型材和光亮產(chǎn)品的交貨技術(shù)條件
|
|
|
|
|
|
|
|
|
|
Chemical comb % of steel X8Cr Ni S18-9 (1.4305): EN 10088-2-2005
|
|
|
|
|
|
|
|
|
|
未經(jīng)買方同意,不得故意將本表中未列出的元素添加到鋼材中,除非對鑄件進(jìn)行精加工。
|
|
|
|
|
|
|
|
|
|
C
|
Si
|
Mn
|
Ni
|
P
|
S
|
Cr
|
N
|
Cu
|
|
max ? 0.1
|
max ? 1
|
max ? 2
|
8月10日
|
max ? 0.045
|
0.15 - 0.35
|
17 - 19
|
max ? 0.11
|
max ? 1
|
|
|
|
|
|
|
|
|
|
|
|
Mechanical properties of ? steel ? X8CrNiS18-9 (1.4305)?
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Rm?- Tensile strength (MPa) (+A)
|
500-700
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Rp0.2?0.2% proof strength (MPa) (+A)
|
190
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
A?- Min. elongation at fracture (%) (+A)
|
35
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
? Brinell hardness ? (HB): ? (+A)
|
230
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Properties of ? steel ? X8CrNiS18-9 (1.4305)
|
|
|
|
|
|
|
|
|
|
Resistance to intergranular corrosion: in the delivery condition - no; in the sensitized condition - no
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Equivalent grades of ? steel ? X8CrNiS18-9 (1.4305)Warning! Only for reference
|
|
|
|
|
|
|
|
|
|
EU?
|
USA
|
Japan
|
France
|
England
|
Sweden
|
|
|
|
|
EN
|
-
|
JIS
|
AFNOR
|
BS
|
SS
|
|
|
|
|
X8CrNiS18-9
|
303
|
SUS303
|
Z8CNF18-09
|
303S31
|
2346?
|
|
|
|
|
|
|
|
|
|
|
|
|
|